The correct and reasonable use of the extruder can give full play to the efficiency of the machine, maintain a good working condition and extend the service life of the machine. The use of screw extruders includes a series of links such as machine installation, adjustment, commissioning, operation, maintenance and repair. Its usage has the common characteristics of general machines, mainly in terms of drive motors and reduction gears. However, the extrusion system has unique characteristics and special attention should be paid to its characteristics when using the pipe extrusion machine. The installation, adjustment and commissioning of the machine are generally clearly specified in the operating instructions of the extruder. The operation methods of the extruder are briefly described below:

1. Preparations before driving
(1) Plastic for extrusion molding. The raw materials should meet the required drying requirements and further drying if necessary. And the raw materials are sieved to remove agglomerates and mechanical impurities.
(2) Check whether the water, electricity and gas systems in the PVC pipe extrusion machine are normal to ensure that the water and gas channels are unobstructed, that the electrical system is normal, that the heating system, temperature control, and various instruments are working reliably; low-speed test of auxiliary equipment empty Run and observe whether the equipment is operating normally; start the vacuum pump of the setting table to observe whether the operation is normal; add lubrication to the smooth parts of various equipment. Remove the fault in time if found.
(3) Install the machine head and setting sleeve. According to the product's variety and size, choose the specifications of the machine head.
2.Drive
(1) You can drive after the temperature is constant. Tighten the bolts of the machine head and the extruder flange again before driving to eliminate the difference in thermal expansion between the bolt and the machine head. Evenly. When tightening the flange nut of the machine head, it is required that the four sides are uniformly tight, otherwise, the material will run away.
(2) When the die is uniformly discharged and has good plasticity, it can be pulled to fix the sleeve. Judgment of plasticization degree needs to be based on experience. Generally, it can be judged according to the appearance of the extruded material, that is, the surface is shiny, free of impurities, non-foaming, charred and discolored. Burrs and cracks have some elasticity, which indicates that the material is plasticized well. If the plasticization is not good, the screw speed, barrel and head temperature can be adjusted appropriately until it meets the requirements.
(3) In the process of extrusion production, it is necessary to regularly check whether the various process parameters are normal according to the process requirements, and fill in the process record sheet. Check the quality of the profile products according to the quality inspection standards, and take timely solutions when problems are found.
3.Parking
(1) Stop feeding and squeeze out the plastic in the PVC pipe extruder. When the screw is exposed, turn off the power of the barrel and the head to stop heating.
(2) Turn off the power of the extruder and auxiliary machine to stop the screw and auxiliary machine.
(3) Open the head flange and remove the head. Clean the perforated plate and various parts of the machine head. In order to prevent damage to the inner surface of the machine head during cleaning, the remaining material in the machine head should be cleaned with steel laws and steel sheets, and then the plastic adhered to the machine head is polished with sandpaper, polished, and coated with oil or silicone rust.